Clear Coating based on XK-258
應用:水性木器無氣噴涂工藝
Pos. | Ingredient | Weight % | Incorporation Method |
1 | XK-258 | 80 | add |
2 | L-RDS(10%, D.W.) | 5 | Addunder stirring |
3 | BYK-022 | 0.4 | 2000rpm/20min |
4 | BYK-028 | 0.8 |
5 | DPnB | 3.2 | mixingboth then add under stirring for 5 mim/1500rpm |
6 | DPM | 2.1 | |
7 | water | 5 |
8 | BYK-347 | 0.5 | Addunder stirring for 5min/1000rpm |
9 | BYK-425(20%,D.W.) | 2 | Addunder stirring for 5min/1000rpm |
10 | water | 1 |
100 |